Skip to main content
Fig. 8 | Materials Theory

Fig. 8

From: Brittle to quasi-brittle transition and crack initiation precursors in crystals with structural Inhomogeneities

Fig. 8

Effect of disorder on average stress: The average stress of the specimens of Lx = 8 μm, Ly = 0.5 mm, and Lz = 1.0. mm where D = 2.995 as a function of the average strain with respect to RG where (a) has a RG = 0.0, (b) has a RG = 0.1, (c). has a RG = 0.2, and (d) has a RG = 0.4. The figure legends signify the notch width W that varies from 0.25 to 128 μm

Back to article page