Fig. 8From: Overdamped langevin dynamics simulations of grain boundary motionHistory of the 5-7 defect pair during the grain shrinkage (dark green) at reduced time a) t=264, b) t=486, c) t=738, d) t=924. Their traces form a regular pattern of hexagonal-shaped cells (for the color code see Fig. 5)Back to article page